Structural adhesives have been part of vehicle assembly for decades. In the body shop, they sit between welded panels and bonded flanges to improve stiffness and spread load evenly across the joint rather than concentrating it at a single weld point. The result is better fatigue resistance over the life of the vehicle.

Structural adhesives are increasingly used to bond dissimilar materials, including metals, plastics, and coated surfaces, in EV battery enclosures and vehicle structures.
Most of what the industry uses falls into one of three chemistries, including acrylics, epoxies, and urethanes. Lap shear strengths run from roughly 7 MPa at the low end of what counts as structural up to around 30 MPa at the high end.
Electric vehicle (EV) battery packs have changed where these materials get used and what they need to do.
The shift started when battery packs grew large enough to need structural bonding the way body panels do. It accelerated with the move from modules inside packs to cell-to-pack and cell-to-chassis designs that fold the adhesive into the vehicle’s load path.
“What’s different now is we’re not using the body shop as our location for adhesives,” said Matt Carroll, principal application engineer with Henkel, during a recent EV Training Day webinar. “We don’t need to worry as much about going through e-coat tanks or high-temperature ovens, but now we need materials that can cure at room temperature and be assembled in general assembly.”
That single change cascades through the rest of the engineering work.
“Adhesives are vital in battery pack architecture, and the technologies are continuously being developed due to evolving application requirements,” he added. “We see structural adhesives playing a more critical role in battery electric vehicles compared to ICE, which makes new innovations even more critical to this market space.”
The chemistry and cure-path framework
Structural adhesives split first by chemistry and second by cure path. Each chemistry brings its own profile of strengths and limitations.
“Acrylics can be very fast acting, but they may have lower temperature resistance and sometimes carry an odor that requires ventilation,” Carroll explained. “Epoxies are the workhorses in the body shop, with high strength and excellent environmental resistance, but they can be brittle unless toughened. Urethanes are known for their high flexibility.”
Urethane formulations can be tailored to different flexibility levels, he said, but they typically need a primer and do not bond as readily as acrylics across all surfaces.
Each of the three chemistries comes in one- or two-component formulations. “A one-part has to cure by baking or moisture exposure,” he said. “A two-part has a curative in one of the components that triggers curing when the two are mixed.”
That distinction used to be unremarkable. In a traditional plant, body-in-white moves from stamping through welding and bonding, then through a paint shop with e-coat tanks and bake ovens before reaching general assembly. The heat of those ovens cured one-component adhesives along the way.
EV battery packs skip that path. Modules and cells arrive in general assembly already, and the adhesive must cure at room temperature once dispensed. That has pushed two-component systems forward as the dominant choice for battery-pack bonding.
A new performance envelope
What battery applications demand of an adhesive sits in a different place from what the body shop demanded. Lightweighting still matters. The materials still must bond dissimilar substrates and hold up across temperature extremes while meeting automotive safety regulations. Several new requirements stack on top of that baseline.

In newer battery-pack designs, adhesives can bond cells directly into the pack structure, reducing the need for intermediate modules.
Flammability is one of the higher-stakes properties. Growing concern about thermal propagation between cells has pulled UL 94 V-0 designations into the adhesive specification for many battery applications, and not every chemistry can hit that target.
Electrical isolation is another consideration. Some products call for measurable resistivity, and others require specific dielectric strength depending on where in the pack the adhesive sits.
Thermal conductivity is the newest addition to the list.
“More recently we’ve looked at the thermal conductance of the adhesives and tried to combine the structural aspect with thermal conductivity, so we can meet a couple of needs at the same time,” Carroll said.
Where a body-shop adhesive only had to bond, a battery adhesive may also need to move heat between the cells it bonds and the cooling plate underneath them.
The packaging environment changed too. Battery enclosures are large, and their dimensional tolerances are looser than what body panels hold. Bond lines vary in thickness more than they would in a stamped joint, which forces the adhesive to perform across a wider gap range without compromising strength.
When adhesives become part of the load path
Early EV battery systems used modules assembled into a pack, and the structural load was carried mostly by the pack enclosure. Cell-to-pack and cell-to-chassis architectures eliminate intermediate structures by bonding cells directly into the larger assembly, which turns the adhesive into a structural element rather than a supporting one.
“We’ve begun seeing a move from modules to packs to cells-to-pack directly integrated,” said Carroll. “Rather than using thermal gap fillers that don’t have as much strength, we’re now seeing more use of thermally conductive adhesives to structurally bond cells and transfer heat from the cells to cooling plates.”
Thermally conductive adhesives are where the new requirements collide most directly.
“These adhesives use fillers that are both thermally conductive and electrically insulative,” he said. “Rather than air between a cell and a cooling plate, which has a thermal conductivity of only 0.02 W/m·K, we now have a polymeric material with fillers around 2 W/m·K, so 100 times more conductive.”
The penalty shows up in mechanical strength. Most thermally conductive products land at the low end of structural, around 7 to 10 MPa lap shear, because the high filler loadings that enable conduction also displace the resin that carries mechanical load. Push thermal conductivity above 2 W/m·K and lap shear typically drops below the structural threshold entirely.
The chemistry mix also changes with the application. “We don’t see too many acrylics in this space,” Carroll added. “In the thermally conductive adhesive world, we’re seeing epoxies and polyurethanes, and these are on the lower limit of structural. The sweet spot for conductivity is mostly 1 to 2 W/m·K.”
Carroll calls the fillers’ double duty “filler magic.”
“We have to find the appropriate fillers for the thermally conductive adhesives, ones that are both conductive yet electrically insulating,” he said. “Even for structural adhesives, there’s a blend of chemistry and filler loadings that play a big role in tailoring the properties.”

Thermally conductive structural adhesives can bond battery cells while also transferring heat to cooling systems, supporting cell-to-pack battery architectures.
The same loading that improves conductivity also needs to remain dielectric. It has to hold its place in the resin during mixing and dispensing without separating over time.
When one property gains, another gives
The combined demand creates a multi-axis tension that no single product satisfies completely. Higher thermal conductivity means more filler. More filler means lower mechanical strength. Stronger flame retardance often comes from additives that work against bond strength. Lower viscosity helps dispensing but can complicate gap filling on uneven surfaces.
“When there’s a desire for higher thermal conductivity, that’s typically handled through higher filler loading, which means more solids and less resin. But that’s usually where you see a drop-off in mechanical strengths,” he shared. “It’s usually like a three-legged stool. You can never be perfect in every area.”
Engineers are left ranking priorities against each other. Which properties get prioritized depends on where in the pack the adhesive sits and which failure mode the design team is most exposed to.
An adhesive between cell and cooling plate prioritizes thermal conductivity and dielectric strength. One at the pack lid favors structural performance and crash response. Inside the module, manufacturing speed often comes first, since the module assembly station tends to be the cycle-time bottleneck.
The conversation between OEMs and adhesive suppliers has changed in response. Adhesives used to arrive as a finished product to be evaluated against a spec. The relationship now starts earlier, with design engineering and materials engineering talking to the supplier’s formulators about what’s possible before the design is locked.
That is the same compression the rest of the EV supply chain has been working through. Development timelines that used to run four or five years now run two or three, and removing iterative loops between design and qualification is the only way to hold that schedule.
For structural adhesive engineering, that earlier conversation may matter as much as the chemistry itself.
“In the past, it was… ‘Here’s the material; now work with it,’” said Carroll. “Now there’s a real conversation, with design engineering, materials engineering, the adhesive formulators, and the manufacturing group all talking about what good looks like and what’s possible from both sides. That’s how you deliver a truly optimized system.”
Filed Under: Adhesives, FAQs