Researchers at Hanyang University ERICA have identified a manufacturing-related defect that may accelerate capacity loss in manganese-stabilized high-nickel cathodes. The cathode design uses a nickel-rich core with a manganese-rich surface layer. This approach could reduce cobalt use while maintaining the energy density needed for electric vehicles (EVs).
A team led by Jin Ho Bang, professor in the Department of Energy and Bio Sciences at Hanyang University ERICA, with PhD candidate JinHa Shim, found that exposure to air during precursor storage can alter the manganese chemistry at the particle surface.
Air exposure oxidized the manganese and contributed to the formation of regions containing Jahn–Teller-distorted manganese species. These surface defects increased reactivity with the electrolyte, leading to electrolyte decomposition and transition-metal dissolution. The reactions also affected the graphite anode.
In the nickel-rich battery systems studied, the defect nearly doubled the rate of capacity fading during extended cycling tests.
“We found that a manganese-rich shell, which is normally introduced to protect high-nickel cathodes, can instead become a catalyst for degradation if the precursor chemistry is not carefully controlled,” said Bang. “Even small variations in precursor storage history can substantially affect battery stability.”
The researchers found that increasing the amount of excess lithium used during synthesis suppressed the defective surface phase and restored more stable manganese-oxygen bonding. The modified cathodes retained more than 90% of their capacity in testing.
The results point to precursor storage and handling as a variable in cathode manufacturing that has received little attention. Controlling lithium stoichiometry during synthesis may offer a way to improve stability without adding another coating process or substantially redesigning production equipment.
“Our results show that even minor variations in precursor history can have major consequences for battery performance, making precursor management an important consideration for large-scale manufacturing,” Bang said.
Reference: The study, “Precursor-driven Jahn–Teller distortion as a hidden origin of surface instability in Mn-stabilized Ni-rich cathodes,” appeared online May 13, 2026, and was published in Volume 19, Issue 12 of Energy & Environmental Science on June 23, 2026.